Material Notes:
Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature ranges, are available. Uses include heat transfer, electronic reliability testing, vapor phase soldering, solvents (especially SV grades), and acid spill mitigation.
Physical Properties Metric English Comments
Density 1.71 g/cc

@Temperature 25.0 °C
0.0618 lb/in³

@Temperature 77.0 °F
Solubility of Water 0.0014 %
0.0014 %
Kinematic Viscosity 0.77 cSt

@Temperature 25.0 °C
0.77 cSt

@Temperature 77.0 °F
Vapor Pressure 0.000947 bar

@Temperature 20.0 °C
0.710 torr

@Temperature 68.0 °F
0.133 bar

@Temperature 60.0 °C
100 torr

@Temperature 140 °F
Thermal Properties Metric English Comments
Heat of Vaporization 66.9 J/g

@Temperature 110 °C
28.8 BTU/lb

@Temperature 230 °F
at boiling point
Boiling Point 110 °C
230 °F
Descriptive Properties Value Comments
Autoignition Temperature (°C) None
Fire Point (°C) None
Flash Point (°C) None
ODP 0
Users viewing this material also viewed the following: