Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Galden® SV55 PFPE Solvent

Category Fluid , Solvent , Polymer
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name Galden®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Galden® SV55 PFPE Solvent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature ranges, are available. Uses include heat transfer, electronic reliability testing, vapor phase soldering, solvents (especially SV grades), and acid spill mitigation.
Physical Properties Metric English Comments
Density 1.65 g/cc

@Temperature 25.0 °C
0.0596 lb/in³

@Temperature 77.0 °F
Solubility of Water 0.0014 %
0.0014 %
Kinematic Viscosity 0.45 cSt

@Temperature 25.0 °C
0.45 cSt

@Temperature 77.0 °F
Vapor Pressure 0.133 bar

@Temperature 9.00 °C
100 torr

@Temperature 48.2 °F
0.304 bar

@Temperature 20.0 °C
228 torr

@Temperature 68.0 °F
1.27 bar

@Temperature 60.0 °C
950 torr

@Temperature 140 °F
Thermal Properties Metric English Comments
Heat of Vaporization 92.0 J/g

@Temperature 55.0 °C
39.6 BTU/lb

@Temperature 131 °F
at boiling point
Boiling Point 55.0 °C
131 °F
Descriptive Properties Value Comments
Autoignition Temperature (°C) None
Fire Point (°C) None
Flash Point (°C) None
ODP 0