Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 1180 cSt @Temperature 25.0 °C |
1180 cSt @Temperature 77.0 °F |
|
Dow VORANOL™ 4815 Polyether Polyol VORANOL™ 4815 polyether polyol is a high reactivity capped triol. Its high molecular weight and high primary hydroxyl content make it well suited for high resiliency, flexible molded foams.Informa.. |