Polymer Property : Viscosity Measure = 1180 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Measure 1180 cSt

@Temperature 25.0 °C
1180 cSt

@Temperature 77.0 °F
Dow VORANOL™ 4815 Polyether Polyol
VORANOL™ 4815 polyether polyol is a high reactivity capped triol. Its high molecular weight and high primary hydroxyl content make it well suited for high resiliency, flexible molded foams.Informa..