Dow VORANOL™ 4815 Polyether Polyol

Category Polymer , Thermoset
Manufacturer Dow Chemical
Trade Name VORANOL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow VORANOL™ 4815 Polyether Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VORANOL™ 4815 polyether polyol is a high reactivity capped triol. Its high molecular weight and high primary hydroxyl content make it well suited for high resiliency, flexible molded foams.Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.017 g/cc
1.017 g/cc
pH 8.8
8.8
(1 Water / 10 Methanol)
Viscosity Measure 86 cSt

@Temperature 98.9 °C
86 cSt

@Temperature 210 °F
680 cSt

@Temperature 37.8 °C
680 cSt

@Temperature 100 °F
1180 cSt

@Temperature 25.0 °C
1180 cSt

@Temperature 77.0 °F
Maximum Moisture Content 0.060
0.060
wt% water
ASTM Color <= 50
<= 50
APHA
Thermal Properties Metric English Comments
Flash Point >= 224 °C
>= 435 °F
Chemical Properties Metric English Comments
Total Acid Number 0.020
0.020
[mg KOH/g]
Descriptive Properties Value Comments
Hydroxyl Number mg KOH/g 28.1