Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.06 - 1.12 g/cc @Temperature 20.0 °C |
0.0383 - 0.0405 lb/in³ @Temperature 68.0 °F |
B Grade |
Kazanorgsintez Purified Polyglycol Production Method: A Grade - Glycol solution in water with mass fraction greater than 75% B Grade - Glycol solution in water with mass fraction greater than 45% Application: A Grade - Intended for .. |
|||
Density | 1.06 g/cc @Temperature 50.0 °C |
0.0383 lb/in³ @Temperature 122 °F |
Concentration 0.08 kg FeCl3/kg |
Solvay Chemicals Ferric chloride Ferric chloride is a red brown aqueous solution, with a slight odor.EINECS: 231-729-4/CAS: 7705-08-0/UN: 2582Information provided by Solvay |
|||
Density | 1.06 g/cc @Temperature 40.0 °C |
0.0383 lb/in³ @Temperature 104 °F |
|
BASF Pluracol® SG-360 Rigid Polyol Description: Pluracol® SG-360 polyol is a clear, light colored, low viscosity, sucrose/glycerine polyol. Pluracol SG-360 contains no nitrogen. The medium functionality polyol, when combined with su.. |