Physical Properties Metric English Comments
Carbon Dioxide Transmission 15.0 cc-mm/m²-24hr-atm
38.1 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® HB 5299 HV PA*
Product description: Grivory HB 5299 HV is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. HV indicates high viscosity, sui..
Carbon Dioxide Transmission 15.0 cc-mm/m²-24hr-atm
38.1 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® HB 5299 HV PA*
Product description: Grivory HB 5299 HV is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. HV indicates high viscosity, sui..
Carbon Dioxide Transmission 15.0 cc-mm/m²-24hr-atm
38.1 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® HB5299 PA*
Product description: Grivory HB 5299 is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. Excellent oxygen and carbon dioxide..
Carbon Dioxide Transmission 15.0 cc-mm/m²-24hr-atm
38.1 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® HB5299 PA*
Product description: Grivory HB 5299 is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. Excellent oxygen and carbon dioxide..