EMS-Grivory Grivory® HB5299 PA*

Category Polymer , Thermoplastic , Nylon
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® HB5299 PA*.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grivory HB 5299 is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. Excellent oxygen and carbon dioxide barrier, especially in interaction with moisture (50 up to 100% relative humidity)Excellent transparency, even for thicker ComponentsSuitable as a middle layer in multi-layer films and componentsSuitable for co-extruded and oriented multilayer films in conjunction with all polyamides, polyesters and polyolefins Barrier properties are not affected by steam sterilization (transparency gets lost) Application: Grivory HB 5299 is used in various multi layer structures providing high barrier (oxygen, carbon dioxide, nitrogen, …), e.g. Co-extrusion blown and cast films.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Water Absorption 5.5 %
5.5 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Water Vapor Transmission 6.00 g/m²/day
0.386 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 4.00 cc/m²/day
0.258 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
4.00 cc/m²/day
0.258 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 15.0 cc-mm/m²-24hr-atm
38.1 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
15.0 cc-mm/m²-24hr-atm
38.1 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
Melt Flow 50 g/10 min
50 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 4.5 %
4.5 %
ISO 527-3
Film Elongation at Break, TD 3.5 %
3.5 %
ISO 527-3
Tensile Modulus 4.00 GPa
580 ksi
dry; ISO 527-1/-2
4.00 GPa
580 ksi
dry; ISO 527-1/-2
Tear Strength 10.0 kN/m
57.1 pli
Trouser Tear resistance MD; ISO 6383-1
10.0 kN/m
57.1 pli
Trouser Tear resistance TD; ISO 6383-1
Elmendorf Tear Strength MD 510 g
510 g
ISO 6383-2
Elmendorf Tear Strength TD 510 g
510 g
ISO 6383-2
Film Tensile Strength at Break, MD 110 MPa
16000 psi
ISO 527-3
Film Tensile Strength at Break, TD 100 MPa
14500 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Gloss 150 %
150 %
60°; ISO 2813
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Packaging Blow moulded containers
Injectionstretchblowmoulded containers
Medical packaging
Non oriented film
Oriented film
Paper coating
Tubes
Processing Blown Film Extrusion
Extrusion - blow molding
Film Extrusion
Other Extrusion
Product Attributes Barrier Properties
High viscosity
Partially aromatic Polyamide
Special Characteristics Transparent