Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 110 - 200 cm³/g | 110 - 200 cm³/g | Average value: 128 cm³/g Grade Count:8 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Viscosity Test | 100 - 200 cm³/g | 100 - 200 cm³/g | Average value: 153 cm³/g Grade Count:4 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |