Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 110 - 200 cm³/g | 110 - 200 cm³/g | Average value: 128 cm³/g Grade Count:8 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Viscosity Test | 110 cm³/g | 110 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by.. |
|||
Viscosity Test | 110 cm³/g | 110 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Viscosity Test | 110 cm³/g | 110 cm³/g | Viscosity number |
BASF Ultradur B 4300 G4 BK5110 20% Glass Filled PBT Ultradur B 4300 G4 BK5110 is an easy flowing, pigmented black, injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Viscosity Test | 110 cm³/g | 110 cm³/g | Viscosity Number |
Arkema Group Lacovyl® PB 1153 i PVC LACOVYL PB 1153 i is a vinyl chloride homopolymer manufactured by microsuspension polymerization process for the preparation of plastisols.It is specially suitable for foam products with medium plas.. |
|||
Viscosity Test | 110 cm³/g | 110 cm³/g | Viscosity Number |
Arkema Group Lacovyl® PB 1202 PVC LACOVYL PB 1202 is a vinyl homopolymer manufactured by microsuspension polymerization process for the preparation of plastisols in particular for chemical foams with low plasticizer content.* MAIN C.. |
|||
Viscosity Test | 110 cm³/g | 110 cm³/g | Viscosity Number |
Arkema Group Lacovyl® PB 1152 C PVC LACOVYL PB 1152 C is a vinyl chloride homopolymer manufactured by microsuspension polymerization process for the preparation of plastisols.It is specially suitable for foam products with medium plas.. |