Polymer Property : Bead Size = 1.20 mm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bead Size 1.20 - 2.50 mm
0.0472 - 0.0984 in
SABIC EPS 760FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 760FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
Bead Size 1.20 - 2.50 mm
0.0472 - 0.0984 in
SABIC EPS 763 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 763 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..
Bead Size 1.20 - 1.50 mm
0.0472 - 0.0591 in
BASF Neopor® P 5200 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of silver-gray foams having a considerably higher ther..