Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 19 g/10 min @Load 21.6 kg, Temperature 190 °C |
19 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE501A BLUE MASTERBATCH BLUE PE 501A is a blue LDPE based masterbatch containing 19% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Blue 15:1.Method of Usage: BLUE PE 501A is designed fo.. |
|||
High Load Melt Index | 19 g/10 min @Load 21.6 kg |
19 g/10 min @Load 47.6 lb |
ISO 1133 |
Total 8183 HDPE, blow molding Applications: cosmetic bottles, pharmaceutical bottles, industrial product containers, chemical packaging, food packagingInformation provided provided by Total Petrochemicals.Total Petrochemicals ac.. |