Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Meilian Chemical PE501A BLUE MASTERBATCH

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Meilian Chemical Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Meilian Chemical PE501A BLUE MASTERBATCH.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BLUE PE 501A is a blue LDPE based masterbatch containing 19% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Blue 15:1.Method of Usage: BLUE PE 501A is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, avoiding pollution and malscattering problems caused by pigment.Range of Application: BLUE PE 501A is designed for use in LDPE, HDPE, LLDPE and PP for production of premium high gloss film with optimum printability.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
High Load Melt Index 19 g/10 min

@Load 21.6 kg,
Temperature 190 °C
19 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Descriptive Properties Value Comments
Carrier LDPE
Compatibility LDPE, HDPE, PP and Ethylene copolymer
Pigment Content 19