Total 8183 HDPE, blow molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Total Atofina
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total 8183 HDPE, blow molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: cosmetic bottles, pharmaceutical bottles, industrial product containers, chemical packaging, food packagingInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D 792
Environmental Stress Crack Resistance 200 hour
200 hour
ASTM D1693 cond. B 10% lgepal
Melt Flow 0.55 g/10 min

@Load 2.16 kg
0.55 g/10 min

@Load 4.76 lb
ISO 1133
1.9 g/10 min

@Load 5.00 kg
1.9 g/10 min

@Load 11.0 lb
ASTM D 1238
High Load Melt Index 19 g/10 min

@Load 21.6 kg
19 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell L 41
41
ASTM D 785
Hardness, Shore D 62
62
ASTM D 2240
Tensile Strength, Yield >= 22.1 MPa
>= 3200 psi
ASTM D 638 type IV
Elongation at Break >= 500 %
>= 500 %
ASTM D 638, type IV
Flexural Modulus 0.965 GPa
140 ksi
ASTM D 790
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
ASTM D 696
Melting Point 129 °C
264 °F
ASTM D3417
Vicat Softening Point 125 °C
257 °F
ASTM D 1525
Copyright © lookpolymers.com All Rights Reserved