Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 15 g/10 min @Load 21.6 kg |
15 g/10 min @Load 47.6 lb |
ISO 1133 |
SIDPEC EGYPTENE® HD 4602 FA HDPE Film Applications:Strong filmTrash bagShopping bagFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., official dis.. |
|||
High Load Melt Index | 15 g/10 min @Load 21.6 kg, Temperature 250 °C |
15 g/10 min @Load 47.6 lb, Temperature 482 °F |
|
BASF Luranyl® KR 2454/3 G4 Polyphenylene Ether + Styrene-Butadiene Blend, 20% Glass Fiber Reinforced Glass fiber reinforced grade containing halogen-free flame-retardant; for moldings with high heat resistance and stiffness (e.g. relay parts, controller and switch housings).Data was collected by IS.. |
|||
High Load Melt Index | 15 - 20 g/10 min @Load 21.6 kg, Temperature 260 °C |
15 - 20 g/10 min @Load 47.6 lb, Temperature 500 °F |
|
Ashley Polymers Ashlene® PC/ABS Alloy 307HF General purpose with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |