Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 15 - 20 g/10 min @Load 21.6 kg, Temperature 260 °C |
15 - 20 g/10 min @Load 47.6 lb, Temperature 500 °F |
|
Ashley Polymers Ashlene® PC/ABS Alloy 307HF General purpose with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |