Nitriflex Nitrilatex NTL-350 Styrene Butadiene Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Nitriflex
Trade Name Nitrilatex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nitriflex Nitrilatex NTL-350 Styrene Butadiene Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesives manufacture, fibers agglomeration, supported gloves manufacture, impregnation of non-woven, etc. Information provided by Dax Resinas
Physical Properties Metric English Comments
Solids Content 49 - 51 %
49 - 51 %
Method L-001/P-065; ASTM D1417
pH 11 - 12
11 - 12
25°C, Method L-003; ASTM D1417
Brookfield Viscosity 70 cP
70 cP
(spindle=1, 20 rpm); ASTM D1417
Surface Tension 35 - 45 dynes/cm
35 - 45 dynes/cm
Method L-005/L-040; ASTM D1417