Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 270 Mesh | 270 Mesh | Opening 1700µm; ASTM E11 |
Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS Some applications of this product may be regulated or restricted by national or international standards (e.g. for food additives, water treatment, the pharmaceutical industry, etc). The buyer and th.. |
|||
Particle Mesh Size | 270 Mesh | 270 Mesh | 97% thru; ASTM D1921B |
Formosa Plastics Formolon® 260 PVC PVC Homopolymer Blending Resin F-260 is a fine particle size PVC homopolymer plastisol blending resin. It combines excellent fusion characteristics, low plastisol viscosities as well as lot to lot u.. |
|||
Particle Mesh Size | 270 Mesh | 270 Mesh | 97% thru; ASTM D1921B |
Formosa Plastics Formolon® 265 PVC PVC Copolymer Blending Resin F-265 is a fine particle size polyvinyl chloride vinyl acetate copolymer plastisol blending resin. The product has been designed for use in application where rapid gelat.. |