Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS

Category Ceramic
Manufacturer Solvay Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Some applications of this product may be regulated or restricted by national or international standards (e.g. for food additives, water treatment, the pharmaceutical industry, etc). The buyer and the eventual user, in his sole and entire liability, shall respect those standards, orders of any relevant authority, and all existing patents and intellectual properties rights; and shall comply with the laws and the regulations applicable to our products and/or to his activity. The buyer and the eventual user must independently determine the suitability of this product for any particular purpose and its manner of use. Please contact us for further information on grades developed for a specific end-use. EINECS Number: 215-185-5/CAS Number: 1310-73-2Information provided by Solvay
Physical Properties Metric English Comments
Particle Mesh Size 10 Mesh
10 Mesh
Opening 2000µm; ASTM E11
12 Mesh
12 Mesh
Opening 1700µm; ASTM E11
14 Mesh
14 Mesh
Opening 1700µm; ASTM E11
16 Mesh
16 Mesh
Opening 1700µm; ASTM E11
18 Mesh
18 Mesh
Opening 1700µm; ASTM E11
20 Mesh
20 Mesh
Opening 1700µm; ASTM E11
25 Mesh
25 Mesh
Opening 1700µm; ASTM E11
30 Mesh
30 Mesh
Opening 1700µm; ASTM E11
35 Mesh
35 Mesh
Opening 1700µm; ASTM E11
40 Mesh
40 Mesh
Opening 1700µm; ASTM E11
45 Mesh
45 Mesh
Opening 1700µm; ASTM E11
50 Mesh
50 Mesh
Opening 1700µm; ASTM E11
60 Mesh
60 Mesh
Opening 1700µm; ASTM E11
70 Mesh
70 Mesh
Opening 1700µm; ASTM E11
80 Mesh
80 Mesh
Opening 1700µm; ASTM E11
100 Mesh
100 Mesh
Opening 1700µm; ASTM E11
120 Mesh
120 Mesh
Opening 1700µm; ASTM E11
140 Mesh
140 Mesh
Opening 1700µm; ASTM E11
170 Mesh
170 Mesh
Opening 1700µm; ASTM E11
200 Mesh
200 Mesh
Opening 1700µm; ASTM E11
230 Mesh
230 Mesh
Opening 1700µm; ASTM E11
270 Mesh
270 Mesh
Opening 1700µm; ASTM E11
325 Mesh
325 Mesh
Opening 1700µm; ASTM E11
400 Mesh
400 Mesh
Opening 1700µm; ASTM E11
Molecular Weight 40.01 g/mol
40.01 g/mol
Descriptive Properties Value Comments
Color White
Composition <0.1 mg/kg
Hg, ISO 5993
<0.5 mg/kg
Pb
<1 mg/kg
Cd
<1 mg/kg
Cr
<10 mg/kg
Fe, ISO 6685
<2 mg/kg
Ni, ISO 11885
<2 mg/kg
As
<200 mg/kg
NaCl, ASTM E1787
<4 g/kg
Na2CO3, ISO 3196
<5 mg/kg
Sb
<5 mg/kg
Se
<80 mg/kg
Na2SO4, ASTM E1787
>990 g/kg
NaOH, ISO 979