Physical Properties Metric English Comments
Brookfield Viscosity 2100 - 2900 cP
2100 - 2900 cP
Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Lubrizol Advanced Materials Pearlstick® D40-70/25 Linear Thermoplastic Polyurethane
Pearlstick D40-70/25 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. ..
Brookfield Viscosity 2500 - 2900 cP
2500 - 2900 cP
Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Lubrizol Advanced Materials Pearlstick® 45-40/27 Polycaprolactone based TPU
Pearlstick 45-40/27 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level.Solubility:..
Brookfield Viscosity 2500 - 2900 cP

@Temperature 25.0 °C
2500 - 2900 cP

@Temperature 77.0 °F
C.O.I.M. EXTER S® S 200 Special Laminate
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 200: Tack-free and h..