Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 2100 - 2900 cP | 2100 - 2900 cP | Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® D40-70/25 Linear Thermoplastic Polyurethane Pearlstick D40-70/25 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. .. |
|||
Brookfield Viscosity | 2500 - 2900 cP | 2500 - 2900 cP | Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 45-40/27 Polycaprolactone based TPU Pearlstick 45-40/27 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level.Solubility:.. |
|||
Brookfield Viscosity | 2500 - 2900 cP @Temperature 25.0 °C |
2500 - 2900 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 200 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 200: Tack-free and h.. |