Polymer Property : Brookfield Viscosity = 2100 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 2100 - 2500 cP

@Temperature 20.0 °C
2100 - 2500 cP

@Temperature 68.0 °F
Brookfield RVF sp. 4, 20 rpm solution at 15% in MEK; MQSA N° 40A
Lubrizol Advanced Materials Pearlstick® 49-46/23 Linear Thermoplastic Polyurethane Elastomer  (discontinued **
Pearlstick 49-46/23 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low thermoplasticity level, available as pellets.Solubility: Pearlstick 49-46/23 is solu..
Brookfield Viscosity <= 2100 cP
<= 2100 cP
Spindle # 4, rpm 60
Michelman® Michem® Dispersion 471 Solvent dispersion of carnauba wax
Description: Solvent dispersion of carnauba waxUsage: Michem® Dispersion 471 provides slip and abrasion resistance. This product has proven very effective for slip and abrasion resistance when us..
Brookfield Viscosity 2100 cP
2100 cP
RVT
Gromax EP-5016M Unplasticized Vinyl Acetate homopolymer
Product Description: EP-5016M is a water redispersible vinyl acetate homopolymer powder that is readily dispersible in water and forms stable emulsion. This redispersible powder is especially recomm..
Brookfield Viscosity 2100 - 2900 cP
2100 - 2900 cP
Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Lubrizol Advanced Materials Pearlstick® D40-70/25 Linear Thermoplastic Polyurethane
Pearlstick D40-70/25 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. ..
Brookfield Viscosity 2100 cP

@Temperature 23.9 °C
2100 cP

@Temperature 75.0 °F
Mixed
BCC Products BC 5009 General Purpose Epoxy System
BC5009 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC5009 is a clear-amber epoxy adhesive especially formulated for the bonding of wood and u..