Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1500 - 2000 cP | 1500 - 2000 cP | resin age: 0-3 months |
Hybrid Plastics Fireban® Mark VII Resorcinolinic (PRF) The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics |
|||
Brookfield Viscosity | 1500 - 5500 cP | 1500 - 5500 cP | DOP 60phr; ASTM D1824 |
LG Chemical PB1302 PVC General Description: PB1302, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for ca.. |
|||
Brookfield Viscosity | <= 1500 cP | <= 1500 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Guard 1351 Nonionic based product of polyethylene wax Description: Nonionic based product of polyethylene waxUsage: Michem® Guard 1351 is a water based dispersion which improves rub and abrasion resistance in pigmented coatings and semi-gloss coatin.. |
|||
Brookfield Viscosity | 1500 cP | 1500 cP | 15% Toluene Solution at 25°C; KM 06 |
Kraton® G1640 E (SEBS) Linear Triblock Copolymer Description: Kraton G1640 E is a clear linear triblock copolymer based on styrene and ethylene/butylene (S-E/B-S) with bound styrene of 32.9% mass. It is supplied from Europe as identified in the gr.. |
|||
Brookfield Viscosity | 1500 cP @Temperature 25.0 °C |
1500 cP @Temperature 77.0 °F |
10% Toluene solution; KM 06 |
Kraton® G1651 E (SEBS) Linear Block Copolymer Description: Kraton G1651 E is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 31.5% mass. It is supplied from Europe in the physical forms .. |
|||
Brookfield Viscosity | 1500 cP | 1500 cP | 10% Toluene Solution at 25°C; KM 06 |
Kraton® G1651 E (SEBS) Linear Triblock Copolymer Description: Kraton G1651 E is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 31.5% mass. It is supplied from Europe in the physical forms .. |
|||
Brookfield Viscosity | 1500 cP @Temperature 125 °C |
1500 cP @Temperature 257 °F |
|
Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: Epolene E-20 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness and low color. It has a low softening point and low viscosity, which give .. |
|||
Brookfield Viscosity | 1500 cP @Temperature 125 °C |
1500 cP @Temperature 257 °F |
|
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: EE-2 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness. It is an excellent asphalt modifier which mixes readily with all asphalts. It h.. |
|||
Brookfield Viscosity | 1500 cP @Temperature 125 °C |
1500 cP @Temperature 257 °F |
|
Westlake Epolene® N-10 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-10 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Brookfield Viscosity | 1500 cP | 1500 cP | RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in Cyclohexanone |
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane Features: High tensile strength, low temperature flexibility, and high adhesion to various substrates such as PET, PVC, and various fabrics.Uses: Fabric coating and audio tape binder, inks and solut.. |
|||
Brookfield Viscosity | 1500 - 4000 cP | 1500 - 4000 cP | RVF #4 sp @ 20 rpm @ 80°F |
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Brookfield Viscosity | 1500 - 3200 cP | 1500 - 3200 cP | RVF #3 sp @ 20 rpm |
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Brookfield Viscosity | 1500 cP @Temperature 25.0 °C |
1500 cP @Temperature 77.0 °F |
Brookfield LVF, Spindle 1-60 RPM |
BCC Products BC 100 Thick Cyanoacrylate Adhesive BC100 Thick is the slow and thickest member of the BCC Products line of cyanoacrylate adhesive. Excellent for gap filling the BC100 Thick has a 30 second fixture time allowing for the material to f.. |
|||
Brookfield Viscosity | 1500 - 3000 cP | 1500 - 3000 cP | Part B, CP#52 @ 100 rpm |
3M Scotch-Weld™ DP600NS Concrete Repair and Self-Leveling 3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600NS is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a tri.. |
|||
Brookfield Viscosity | 1500 - 3000 cP | 1500 - 3000 cP | Part B, CP #52 @ 100 rpm |
3M Scotch-Weld™ DP601NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon.. |
|||
Brookfield Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | RVT #2 spindle @ 20 rpm |
3M Scotch-Weld™ RT35 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |