Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High tensile strength, low temperature flexibility, and high adhesion to various substrates such as PET, PVC, and various fabrics.Uses: Fabric coating and audio tape binder, inks and solution cast pigment dispersion media Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Brookfield Viscosity 200 cP
200 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in MEK
1500 cP
1500 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in Cyclohexanone
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength 50.3 MPa
7300 psi
ASTM D412/D638
Elongation at Break 430 %
430 %
ASTM D412/D638
100% Modulus 0.00230 GPa
0.334 ksi
ASTM D412/D638
300% Modulus 0.00590 GPa
0.856 ksi
ASTM D412/D638
Peel Strength 0.260 kN/m
1.48 pli
Adhesion to PET; TP-141
Thermal Properties Metric English Comments
Vicat Softening Point 35.0 °C
95.0 °F
ASTM D1525
Glass Transition Temp, Tg 19.0 °C
66.2 °F
DSC