Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Westlake Chemical Corporation
Trade Name Epolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Epolene E-20 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness and low color. It has a low softening point and low viscosity, which give it the same desirable emulsification properties of a low-density oxidized polyethylene. The low softening point and low viscosity contribute to the hardness, short drying time, and excellent gloss in coatings. Pressure equipment is required for mulsification of this material. Epolene E-20 is an excellent performer in high-speed, buffable floor finishes. It improves buffability and durability.Key Attributes:Imparts slip resistance, durability, and toughness to floor finishes Low density polyethylene (PE)Oxidized to provide functionalityProduces stable water based emulsions Useful as a lubricant for HDPE extrusionApplication/Uses: Automotive Building and ConstructionHot Melt AdhesivesPressure Sensitive AdhesivesSolventborne AdhesivesWaterborne AdhesivesWax Modification
Physical Properties Metric English Comments
Specific Gravity 0.930 - 0.960 g/cc
0.930 - 0.960 g/cc
Viscosity 1000 - 2000 cP

@Temperature 125 °C
1000 - 2000 cP

@Temperature 257 °F
542-111
Brookfield Viscosity 1500 cP

@Temperature 125 °C
1500 cP

@Temperature 257 °F
Molecular Weight 7500 g/mol
7500 g/mol
Thermal Properties Metric English Comments
Flash Point >= 204 °C
>= 399 °F
Ring & Ball Softening Point 111 °C
232 °F
ASTM E28
Optical Properties Metric English Comments
Gardner Color Number <= 2.0
<= 2.0
542-130
Chemical Properties Metric English Comments
Total Acid Number 17
17
Descriptive Properties Value Comments
Penetration Hardness <1 dmm
ASTM D5, Needle under 100-g load for 5s @ 25 deg C, tenths of mm