Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 140 cP @Temperature 25.0 °C |
140 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya OMYAFLOW® 3 - SY Calcium Carbonate A beneficiated calcium carbonate with excellent fineness, color, and dispersion characteristics available in dry and slurry forms.Applications: Decorative paints.Information supplied by Omya North A.. |
|||
Brookfield Viscosity | 140 - 220 cP | 140 - 220 cP | |
LG Chemical CP-WB Polycarboxylic Copolymer Description: CP-WB is the main raw material for concrete admixture, which improves water reducing and slump retention abilities. CP-WB was developed through our advanced synthetic technologies, impa.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® A 11 Acrylic polymer dispersion Licomer® A 11 is an aqueous polymer dispersion suitable for the manufacture of products for the finishing of shoes and leather. This product provides excellent gloss and flexibility, and provides.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® A 41 Styrene-Acrylate copolymer dispersion Description: Styrene-Acrylate copolymer dispersionUsage: Licomer® A 41 is an aqueous polymer dispersion for dry bright emulsions for household floors, shoes and leather products to provide high g.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® A 53 Acrylic polymer dispersion Description: Acrylic polymer dispersionUsage: Licomer® A 53 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the care of floors. This product p.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® A 623 Styrene - Acrylate copolymer dispersion Description: Styrene - Acrylate copolymer dispersionUsage: Licomer® A 623 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the care of floors. .. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® A 65 Styrene - Acrylate copolymer dispersion Description: Styrene - Acrylate copolymer dispersionUsage: Licomer® A 65 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the care of floors. T.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® IN 41 Anionic / Nonionic polyethylene emulsion Description: Anionic / Nonionic polyethylene emulsionUsage: Licomer® IN 41 is a high anti-slip additive for floor polish formulations.Information provided by Michelman® |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® M 36 Styrene-Acrylate copolymer dispersion Description: Styrene-Acrylate copolymer dispersion, metal containingUsage: Licomer® M 36 is suitable for easy removal dry-bright emulsions and provides a film with good resistance to alcohol.Info.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® R 20 Ammonia solution of a rosin, modified with maleic acid Description: Ammonia solution of a rosin, modified with maleic acidUsage: Licomer® R 20 is an additive for floor polish formulations.Information provided by Michelman® |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® T 51 Acrylic copolymer dispersion Description: Acrylic copolymer dispersion, metal containingUsage: Licomer® T 51 is a dispersion suitable for dry-bright emulsions and cleaning products due to high transparency and hardness. This.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® W 11 Anionic / Nonionic polyethylene emulsion Description: Anionic / Nonionic polyethylene emulsionUsage: Licomer® W 11 is an emulsion designed for floor polish formulations providing high hardness and gloss. This emulsion forms a clear film.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® W 19 Anionic / Nonionic polyethylene emulsion Description: Anionic / Nonionic polyethylene emulsionUsage: Licomer® W 19 is an emulsion designed for floor polish formulations providing high hardness and gloss. This emulsion forms a clear film.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® W 315 FP Anionic / Nonionic polyethylene emulsion Description: Anionic / Nonionic polyethylene emulsionUsage: Licomer® W 315 FP is a high anti-slip emulsion suitable for floors, finishes on shoes, leather, etc.Information provided by MichelmanÂ.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® W 483 Nonionic montan emulsion Description: Nonionic montan emulsionUsage: Licomer® W 483 is a high gloss concentrated emulsion, used for dry-bright polishes.Information provided by Michelman® |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® W 485 Cationic montan emulsion Description: Cationic montan emulsionUsage: Licomer® W 485 is a high gloss emulsion that improves the performance of floor crystalllizers.Information provided by Michelman® |
|||
Brookfield Viscosity | 140 - 220 cP @Temperature 25.0 °C |
140 - 220 cP @Temperature 77.0 °F |
25% Toluene solution |
Kraton® G1726 M (SEBS) Linear Copolymer Description: Kraton G1726 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® M 55 Styrene-Acrylate copolymer dispersion Description: Styrene-Acrylate copolymer dispersion, metal containingUsage: Licomer® M 55 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the c.. |
|||
Brookfield Viscosity | <= 140 cP | <= 140 cP | |
Michelman® Licomer® M 63 Styrene-Acrylate copolymer dispersion Description: Styrene-Acrylate copolymer dispersion, metal containingUsage: Licomer® M 63 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the c.. |
|||
Brookfield Viscosity | 140 cP @Temperature 200 °C |
140 cP @Temperature 392 °F |
Melt |
Zeon Chemicals Quintone® C200S Aliphatic Hydrocarbon Resin C5 type (piperylene precursor). Has excellent flowability, heat stability and colors, suitable for traffic paint.Information provided by Zeon Chemicals L.P. |