Michelman® Licomer® W 19 Anionic / Nonionic polyethylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Licomer®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Licomer® W 19 Anionic / Nonionic polyethylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Anionic / Nonionic polyethylene emulsionUsage: Licomer® W 19 is an emulsion designed for floor polish formulations providing high hardness and gloss. This emulsion forms a clear film and also provides excellent abrasion resistance, water resistance and excellent resistance to scratching. Licomer® W 19 is also suitable for flexographic printing lacquers and inks for improved resistance to rubbing and scratching.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.02 g/cc
1.00 - 1.02 g/cc
Volatiles 64 - 66 %
64 - 66 %
pH 9.0 - 10.5
9.0 - 10.5
Brookfield Viscosity <= 140 cP
<= 140 cP
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Light yellow liquid
Emulsifier Charge Anionic/Nonionic
Solids Type Polyethylene