Michelman® Licomer® W 315 FP Anionic / Nonionic polyethylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Licomer®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Licomer® W 315 FP Anionic / Nonionic polyethylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Anionic / Nonionic polyethylene emulsionUsage: Licomer® W 315 FP is a high anti-slip emulsion suitable for floors, finishes on shoes, leather, etc.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.00 g/cc
0.990 - 1.00 g/cc
Volatiles 81 - 83 %
81 - 83 %
pH 8.0 - 9.5
8.0 - 9.5
Brookfield Viscosity <= 140 cP
<= 140 cP
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance White liquid
Emulsifier Charge Anionic/Nonionic
Solids Type Polyethylene