Polymer Property : Environmental Stress Crack Resistance = 250 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Environmental Stress Crack Resistance >= 250 hour
>= 250 hour
ISO 22088
Polimeri Europa Clearflex® RN 50 U Linear Medium Density Polyethylene
Clearflex RN 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha..
Environmental Stress Crack Resistance >= 250 hour
>= 250 hour
ASTM D1693
NIZHNEKAMSKNEFTEKHIM PE 6751E (516H5) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Environmental Stress Crack Resistance 250 hour
250 hour
F50, Igepal, Condition C; ASTM D-1693
ExxonMobil Escorene® LL-5102 LLDPE Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL-5102 makes for effici..
Environmental Stress Crack Resistance 250 hour
250 hour
F50, Condition A, ASTM D1693, 100% Igepal
NOVA Chemicals Sclair® 8405 BK, 8405GBK MDPE Rotational Molding Resin  (discontinued **)
Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer.
Environmental Stress Crack Resistance 250 hour
250 hour
F50, Condition A, ASTM D1693, 100% Igepal
NOVA Chemicals Sclair® 8405 UV8D, 8405G UV8D MDPE Rotational Molding Resin  (discontinued **)
Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer.
Environmental Stress Crack Resistance >= 250 hour

@Temperature 50.0 °C
>= 250 hour

@Temperature 122 °F
Igepal 100%; F20; ASTM D1693-B
Borealis ME6032 Polypropylene
ME6032 is a MDPE compound for solid insulation of telephone singles and data cables at high line speed. It contains a metal deactivator. Applications: Dry core and petroleum jelly filled cables. S..
Environmental Stress Crack Resistance >= 250 hour
>= 250 hour
100% ant.; ASTM D1693-70
Total 49080 UV HDPE blow molding
FINATHENE® 49080 UV is produced by the slurry loop low pressure polymerization process. FINATHENE® 49080 UV is a U.V.-stabilized, high molecular weight pelletized resin, intended for the productio..
Environmental Stress Crack Resistance >= 250 hour
>= 250 hour
F50, Anatarox 100%; ASTM D 1693B
Total HDPE 56020 S XP High Density Polyethylene - Blow Molding
HDPE 56020 S XP is a very high molecular weight (VHMW) high density polyethylene with a high resistance to impact, good chemical resistance and optimized balance between Environmental Stress Crack R..
Environmental Stress Crack Resistance >= 250 hour
>= 250 hour
ASTM D1693-70
Total ESD 201 B HDPE blow molding
FINATHENE® ESD 201 B is a black conductive compound manufactured from high performance Finathene high density polyethylene. The use of this HDPE compound gives outstanding compatibility to (semi) h..
Environmental Stress Crack Resistance >= 250 hour
>= 250 hour
ASTM D1693-70
Total Finathene® SI 508 HDPE blow molding  (discontinued **)
Finathene® SI 508 is part of a new generation of high density ethylene-hexene copolymers produced by the slurry loop low pressure polymerization process. Finathene® SI 508 is a high molecular weig..