Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Clearflex® RN 50 U Linear Medium Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Clearflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Clearflex® RN 50 U Linear Medium Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clearflex RN 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mechanical properties and excellent surface aspect.Main Applications: Thanks to high processability, Clearflex RN 50 U is recommended for the production of items with difficult shapes, vases and garden articles.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.936 g/cc
0.936 g/cc
ISO 1183
Environmental Stress Crack Resistance >= 250 hour
>= 250 hour
ISO 22088
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
ISO 868/A
Tensile Strength at Break 17.0 MPa
2470 psi
ISO 527
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527
Elongation at Break >= 700 %
>= 700 %
ISO 527
Flexural Modulus 0.650 GPa
94.3 ksi
ISO 178
Dart Drop Total Energy 210 J/cm
0.393 ft-lb/mil
rotomolded sample; ISO 6603/2
Thermal Properties Metric English Comments
Melting Point 127 °C
261 °F
Internal method
Vicat Softening Point 113 °C

@Load 1.00 kg
235 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Users viewing this material also viewed the following: