Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 650 cc/m²/day @Temperature 23.0 °C |
41.9 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Bicor™ 35MB666 OPP Film Product Description: A is a biaxially oriented transparent polypropylene film, acrylic coated tow sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle E.. |
|||
Oxygen Transmission Rate | 650 cc/m²/day @Temperature 23.0 °C |
41.9 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 52MH647 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Ava.. |
|||
Oxygen Transmission Rate | 650 cc/m²/day @Temperature 23.0 °C |
41.9 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 52MH648 OPP Film Product Description: A high speed super white opaque, modified higher density, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS.. |
|||
Oxygen Transmission Rate | 650 cc/m²/day @Temperature 23.0 °C |
41.9 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 52MHR647 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented PP film, humidity resistant acrylic coated two sides. This film is designed to wrap products with a high moistu.. |