Physical Properties Metric English Comments
Oxygen Transmission 53.0 - 64.0 cc-mm/m²-24hr-atm
135 - 163 cc-mil/100 in²-24hr-atm
Average value: 58.0 cc-mm/m²-24hr-atm Grade Count:6
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..