Oxygen Transmission 53.0 cc-mm/m²-24hr-atm
135 cc-mil/100 in²-24hr-atm
Air permeation rate @ 23°C (73°F), (ASTM D 1434)
Advanced Elastomer Systems Trefsin® 3101-85 W305 Thermoplastic Rubber  (discontinued **)
A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec..
Oxygen Transmission 53.0 cc-mm/m²-24hr-atm
135 cc-mil/100 in²-24hr-atm
Air permeation rate @ 23°C (73°F), (ASTM D 1434)
Advanced Elastomer Systems Trefsin® 3201-85 W305 Thermoplastic Rubber  (discontinued **)
A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t..
Oxygen Transmission 53.0 - 64.0 cc-mm/m²-24hr-atm
135 - 163 cc-mil/100 in²-24hr-atm
Average value: 58.0 cc-mm/m²-24hr-atm Grade Count:6
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..