Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 53.0 cc-mm/m²-24hr-atm | 135 cc-mil/100 in²-24hr-atm | Air permeation rate @ 23°C (73°F), (ASTM D 1434) |
Advanced Elastomer Systems Trefsin® 3101-85 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |
|||
Oxygen Transmission | 53.0 cc-mm/m²-24hr-atm | 135 cc-mil/100 in²-24hr-atm | Air permeation rate @ 23°C (73°F), (ASTM D 1434) |
Advanced Elastomer Systems Trefsin® 3201-85 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
Oxygen Transmission | 53.0 - 64.0 cc-mm/m²-24hr-atm | 135 - 163 cc-mil/100 in²-24hr-atm | Average value: 58.0 cc-mm/m²-24hr-atm Grade Count:6 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |