Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 197 - 200 cc-mm/m²-24hr-atm | 500 - 508 cc-mil/100 in²-24hr-atm | Average value: 199 cc-mm/m²-24hr-atm Grade Count:5 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |