Physical Properties Metric English Comments
Oxygen Transmission 2.36 cc-mm/m²-24hr-atm
5.99 cc-mil/100 in²-24hr-atm
Tested per ASTM D3985 at 22°C
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 100 Gauge
Data provided by DuPont Packaging Polymers.Mylar® OL13 (formerly known as XM110) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat seal..
Oxygen Transmission 2.36 cc-mm/m²-24hr-atm
5.99 cc-mil/100 in²-24hr-atm
Tested per ASTM D3985 at 22°C
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 100 Gauge
Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a ..
Oxygen Transmission 2.36 cc-mm/m²-24hr-atm
5.99 cc-mil/100 in²-24hr-atm
Tested per ASTM D3985 at 22°C
DuPont Teijin Films Mylar® RL4 Polyester Packaging Film, 100 Gauge
Data provided by DuPont Packaging Polymers.Mylar® RL4 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film ..