Polymer Property : Melt Flow = 78 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 78 g/10 min

@Load 10.0 kg,
Temperature 220 °C
78 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® INP564 ABS
SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Melt Flow 78 g/10 min

@Load 10.0 kg,
Temperature 220 °C
78 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® INP564 ABS+SAN
SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Melt Flow 78 g/10 min

@Load 10.0 kg,
Temperature 220 °C
78 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® INP576 ABS
Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc..
Melt Flow 78 g/10 min

@Load 10.0 kg,
Temperature 220 °C
78 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® INP576 ABS+SAN
Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc..
Melt Flow 78 g/10 min

@Load 10.0 kg,
Temperature 220 °C
78 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East)
CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri..
Melt Flow 78 g/10 min

@Load 1.20 kg,
Temperature 300 °C
78 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Procedure A Condition 0; ASTM D1238
Network Polymers NPP 808 C2WW
Description: Polycarbonate AlloyInformation provided by Network Polymers Inc.
Melt Flow 78 g/10 min

@Load 1.20 kg,
Temperature 300 °C
78 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Procedure A Condition 0; ASTM D1238
Network Polymers NPP 908
Description: Polyester CopolymerInformation provided by Network Polymers Inc.
Melt Flow 78 - 96 g/10 min

@Load 21.6 kg,
Temperature 190 °C
78 - 96 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4116Q (16403) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 78 - 96 g/10 min

@Load 21.6 kg,
Temperature 190 °C
78 - 96 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4118Q (18403) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 78 g/10 min

@Pressure 0.655 MPa
78 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® 1010
PolyOne Geon™ 120 Series 129 Polyvinyl Chloride Homopolymer
The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging..
Melt Flow 78 - 96 g/10 min

@Load 21.6 kg,
Temperature 190 °C
78 - 96 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4318Q (18403) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 78 g/10 min

@Load 1.20 kg,
Temperature 300 °C
78 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Diamond Polymers NPP 60-908 Polyester Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 78 g/10 min

@Load 1.20 kg,
Temperature 300 °C
78 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Diamond Polymers NPP 808 C2 Polycarbonate Alloy, Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 78 g/10 min

@Load 1.20 kg,
Temperature 300 °C
78 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Diamond Polymers NPP 808 C2 TDS Polycarbonate Alloy, Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.