Physical Properties Metric English Comments
Melt Flow 5.2 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.2 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
SABIC Innovative Plastics Geloy XTWE265 ASA
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 5.2 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.2 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 5.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Ravago Manufacturing Americas Hylac® FR134 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Melt Flow 5.2 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.2 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM-D1238, ISO 1133
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade
Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components.
Melt Flow 5.2 g/10 min

@Load 6.60 kg,
Temperature 337 °C
5.2 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
Melt Flow 5.2 g/10 min

@Load 5.00 kg,
Temperature 265 °C
5.2 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Diamond Polymers ABSPC 9901B ABS/PC Blow Molding Grade, High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 5.2 g/10 min

@Load 5.00 kg,
Temperature 265 °C
5.2 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Diamond Polymers ABSPC 9901B-50148 ABS/PC Blow Molding Grade, High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 5.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Chi Mei Polylac® PA-765 ABS - Flame Retardant
F.R. High Flow
Melt Flow 5.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET  (Unverified Data**)
Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various..
Melt Flow 5.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET  (Unverified Data**)
Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various..