Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.80 - 1.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
±15% |
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Melt Flow | 1.2 - 1.6 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.2 - 1.6 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
Forever Plast Namtene® Recycled Standard HDPE Standard Namtene® is used for dimple sheet, plastic slabs, and agricultural and construction applications. |