Polymer Property : Melt Flow = 1.2 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 1.2 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.2 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
SABIC Innovative Plastics Cycolac® MG29 ABS
Super high impact ABS. Good low temperature toughness. High gloss.
Melt Flow 1.2 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.2 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
SABIC Innovative Plastics Cycolac® MG29 ABS (Asia Pacific)
Super high impact ABS. Good low temperature toughness. High gloss.
Melt Flow 1.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound
PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Melt Flow 1.2 - 1.9 g/10 min

@Load 5.00 kg,
Temperature 230 °C
1.2 - 1.9 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PP 8332C (EPD60R) Propylene and Ethylene Block Polymer
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r..
Melt Flow 1.2 g/10 min

@Load 5.00 kg,
Temperature 230 °C
1.2 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer  (discontinued **)
Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina..
Melt Flow 1.2 g/10 min

@Load 5.00 kg,
Temperature 230 °C
1.2 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer  (discontinued **)
Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i..
Melt Flow 1.2 - 1.6 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.2 - 1.6 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Forever Plast Namtene® Recycled Standard HDPE
Standard Namtene® is used for dimple sheet, plastic slabs, and agricultural and construction applications.
Melt Flow 1.2 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.2 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) BL3 HF 4760 High Density Polyethylene
BL3 is a high density polyethylene with 1-Butene as co monomer. It is high density and stiffness, good ESCR, high rigidity, good flowability and impact strength.Applications: small blow molding, bo..
Melt Flow 1.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Kingfa FRABS V-0 Flame Retardant ABS
Features:UL 94 V-0 @ 1.5-3.0mmHigh toughnessFor extrusion moldingApplications:PlateElectric and electronic cabinetPCB boardInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Flow 1.2 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.2 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Borealis Borstar® FB3450 HDPE for Film Extrusion
Borstar® FB3450 is a high density polyethylene. Borstar® FB3450 is well suited for multilayer coextruded films where higher stiffness and toughness than in standard LDPE and LLDPE is required. Ap..
Melt Flow 1.2 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.2 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Unipetrol PE HD LITEN® BB 29 H HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Melt Flow 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Total HDPE BM961 High Density Polyethylene, High Gloss Blow Molding Resin
Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p..
Melt Flow 1.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Chi Mei Polylac® PA-747 ABS
High impact
Melt Flow 1.2 g/10 min

@Load 10.0 kg,
Temperature 220 °C
1.2 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Procedure A; ASTM D1238
Diamond Polymers ABS 3003 MC
Description: High Heat Plating GradeInformation provided by Diamond Polymers, Inc.
Melt Flow 1.2 g/10 min

@Load 5.00 kg,
Temperature 265 °C
1.2 g/10 min

@Load 11.0 lb,
Temperature 509 °F
Procedure A; ASTM D1238
Diamond Polymers ABS 4011 HH
Description: Ultra High Heat ABSInformation provided by Diamond Polymers, Inc.
Melt Flow 1.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 9502
Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 1.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS/PC 7901
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 1.2 g/10 min

@Load 5.00 kg,
Temperature 230 °C
1.2 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Carmel Olefins CARMELTECH™ QB 79 P Polypropylene Random Copolymer for Pressure Pipe
CARMELTECH™ QB 79 P is a high molecular weight, low melt flow rate polypropylene random copolymer, especially designed for extrusion of pressure pipes and injection molding of fittings. This grade ..