Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.90 - 1.5 g/10 min @Load 5.00 kg, Temperature 230 °C |
0.90 - 1.5 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 1532B (YD50G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Melt Flow | 0.90 - 1.5 g/10 min @Load 5.00 kg, Temperature 230 °C |
0.90 - 1.5 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 4132B (PA14D) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates very high long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 1.0 - 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.0 - 1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR Plus High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 1.0 - 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.0 - 1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR Plus T10 High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 1.0 - 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.0 - 1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR Plus T15 High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 1.0 - 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.0 - 1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR White F High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 1.0 - 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.0 - 1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR White F60 High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |