Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.90 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.90 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® BC 82 High Density Polyethylene - Blow Molding Eraclene BC 82 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er.. |
|||
Melt Flow | 0.90 - 1.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 - 1.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.90 - 1.5 g/10 min @Load 5.00 kg, Temperature 230 °C |
0.90 - 1.5 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 1532B (YD50G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Melt Flow | 0.90 - 1.5 g/10 min @Load 5.00 kg, Temperature 230 °C |
0.90 - 1.5 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 4132B (PA14D) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates very high long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 0.90 - 1.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 - 1.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.90 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.90 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® FB2230 LLDPE for Film Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from .. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg |
0.90 g/10 min @Load 4.76 lb |
ISO 1133 |
Total Lumicene® M 3410 EP HDPE Film, sheet FINACENE® M 3410 EP is a medium density metallocene based polyethylene resin. FINACENE® M 3410 EP is especially dedicated to film applications where a higher rigidity, good transparency and shrink.. |
|||
Melt Flow | 0.90 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.90 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133/T |
Total MDPE 3802 B Medium Density Polyethylene, Cable MDPE 3802 B is a black medium density polyethylene particularly suited for cable sheathing applications and designed to meet the requirements for telecommunication and power cables (medium and high .. |
|||
Melt Flow | 0.90 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.90 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133/T |
Total MDPE 3802 Medium Density Polyethylene, Cable MDPE 3802 is a natural medium density polyethylene particularly suited for colored cable sheathing applications and designed to meet the requirements for telecommunication and power cables (medium a.. |
|||
Melt Flow | 0.90 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.90 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® FB2310 LLDPE for Film Borstar BF2310 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from .. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Film Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityExcellent tear strengthHigh puncture resistanceGood stiffnessExcellent heat sealing proper.. |
|||
Melt Flow | 0.90 g/10 min @Load 3.80 kg, Temperature 230 °C |
0.90 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 7500E Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.90 g/10 min @Load 10.0 kg, Temperature 220 °C |
0.90 g/10 min @Load 22.0 lb, Temperature 428 °F |
Procedure A; ASTM D1238 |
Diamond Polymers ABS TR-7 Description: High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.90 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.90 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS VP-11 ELG Description: Extrusion Grade, Low Gloss, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.90 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.90 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA S190 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.90 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.90 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA S750 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.90 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.90 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA S910 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® HTR8341G BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Slightly Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin
(Unverified Data**) Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p.. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total Lumicene® mPE BM359 SG Metallocene Medium Density High Gloss Blow Molding Resin Metallocene Medium Density High Gloss Blow Molding ResinCharacteristics:Outstanding glossGood flexibilityExcellent impact strengthGood ESCRUSP Class VI compliantFDA CompliantApplications:Coextruded .. |