Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NIZHNEKAMSKNEFTEKHIM PP 4132B (PA14D) Propylene and Ethylene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , Polypropylene (PP)
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PP 4132B (PA14D) Propylene and Ethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates very high long-term thermal stability, thermal-oxidative degradation resistance when PP is produced, processed and PP-made articles are exploited.Information provided by manufacturer
Physical Properties Metric English Comments
Melt Flow 0.20 - 0.40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.20 - 0.40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
0.40 - 0.70 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 - 0.70 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238/L
0.90 - 1.5 g/10 min

@Load 5.00 kg,
Temperature 230 °C
0.90 - 1.5 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238/L
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 27.0 MPa
>= 3920 psi
ASTM D638
Elongation at Yield >= 11 %
>= 11 %
ASTM D638
Flexural Modulus >= 0.850 GPa
>= 123 ksi
ASTM D790
Izod Impact, Notched >= 0.400 J/cm

@Temperature -20.0 °C
>= 0.749 ft-lb/in

@Temperature -4.00 °F
ASTM D256