Polymer Property : Oxygen Transmission Rate = 3.86 cc/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 40.0 - 60.0 cc/m²/day
2.58 - 3.86 cc/100 in²/day
400 µm; ASTM F1927-98
Stanelco Bioplast® GS 2189 Biodegradable Plastic
Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable i..