Polymer Property : Oxygen Transmission Rate = 40.0 cc/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 40.0 - 60.0 cc/m²/day
2.58 - 3.86 cc/100 in²/day
400 µm; ASTM F1927-98
Stanelco Bioplast® GS 2189 Biodegradable Plastic
Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable i..
Oxygen Transmission Rate 40.0 cc/m²/day
2.58 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® FG 40 NL nat 6018 PA6
Information provided by EMS Grivory
Oxygen Transmission Rate 40.0 cc/m²/day
2.58 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® FG 47 NL nat 6028 PA6
Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements..
Oxygen Transmission Rate 40.0 - 1000 cc/m²/day
2.58 - 64.4 cc/100 in²/day
Average value: 292 cc/m²/day Grade Count:6
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..
Oxygen Transmission Rate >= 40.0 cc/m²/day
>= 2.58 cc/100 in²/day
25°C, 1.0 µm, 85% RH
Solvay Specialty Polymers Diofan® A610 Polyvinylidene Chloride (PVDC)  (discontinued **)
DIOFAN® A610 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. It features exceptional barrier..