Polymer Property : Water Vapor Transmission = 7.50 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 0.900 - 7.50 g/m²/day
0.0580 - 0.483 g/100 in²/day
Average value: 4.14 g/m²/day Grade Count:8
Overview of materials for PVC, Foam Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma..
Water Vapor Transmission 4.30 - 7.50 g/m²/day
0.277 - 0.483 g/100 in²/day
Average value: 5.78 g/m²/day Grade Count:6
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..