Physical Properties Metric English Comments
Water Vapor Transmission 0.900 - 7.50 g/m²/day
0.0580 - 0.483 g/100 in²/day
Average value: 4.14 g/m²/day Grade Count:8
Overview of materials for PVC, Foam Grade