Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 4.30 g/m²/day | 0.277 g/100 in²/day | 24 hrs, 37.8°C, 90% R.H.; ASTM E96 |
Petromont 2200 High Density Polyethylene Resin Pétromont HDPE 2200 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This resin can be used in a mono layer or co-extrusion resin in applications requiring impr.. |
|||
Water Vapor Transmission | 4.30 g/m²/day | 0.277 g/100 in²/day | 100% Humidity; ASTM F372 |
LyondellBasell Plexar® PX2049 Extrudable Tie-Layer Resin - Anhydride Modified HDPE
(discontinued **) General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Water Vapor Transmission | 4.30 - 7.50 g/m²/day | 0.277 - 0.483 g/100 in²/day | Average value: 5.78 g/m²/day Grade Count:6 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Water Vapor Transmission | 4.30 g/m²/day | 0.277 g/100 in²/day | ASTM F372 |
LyondellBasell Plexar® PX3243 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s.. |
|||
Water Vapor Transmission | 4.30 g/m²/day | 0.277 g/100 in²/day | 38°C, 90% RH; ExxonMobil Method |
ExxonMobil Bicor® 120 CSR-2 OPP Film Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and .. |
|||
Water Vapor Transmission | 4.30 g/m²/day | 0.277 g/100 in²/day | 38°C, 90% RH; ExxonMobil Method |
ExxonMobil Bicor® 120 SLP OPP Film Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin.. |