Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 80.0 - 120 g/m²/day @Thickness 0.0600 mm |
5.15 - 7.73 g/100 in²/day @Thickness 0.00236 in |
film; JIS Z0208 |
Kaneka PHBH Rigid Bio-based Polymer A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions.. |
|||
Water Vapor Transmission | 80.0 - 120 g/m²/day @Thickness 0.0600 mm |
5.15 - 7.73 g/100 in²/day @Thickness 0.00236 in |
film; JIS Z0208 |
Kaneka PHBH Semi-Rigid Bio-based Polymer A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions.. |
|||
Water Vapor Transmission | 80.0 - 150 g/m²/day | 5.15 - 9.66 g/100 in²/day | DIN EN 12086 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Water Vapor Transmission | 80.0 - 200 g/m²/day | 5.15 - 12.9 g/100 in²/day | DIN EN 12086 |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |