Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 50.0 - 150 g/m²/day | 3.22 - 9.66 g/100 in²/day | DIN EN 12086 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Water Vapor Transmission | 80.0 - 150 g/m²/day | 5.15 - 9.66 g/100 in²/day | DIN EN 12086 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Water Vapor Transmission | 100 - 150 g/m²/day | 6.44 - 9.66 g/100 in²/day | DIN EN 12086 |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Water Vapor Transmission | 100 - 150 g/m²/day | 6.44 - 9.66 g/100 in²/day | DIN EN 12086 |
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |
|||
Water Vapor Transmission | 100 - 150 g/m²/day | 6.44 - 9.66 g/100 in²/day | DIN EN 12086 |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |